Detecting Voids in Voided Post-Tensioned Concrete Decks

  • Detecting Voids in Voided Post-Tensioned Concrete Decks

    Posted by jaden on 28/11/2021 at 5:40 pm

    Would anyone be able to give me assistance in contacting
    an expert/company, preferably in Eastern Canada, who
    has experience detecting voids in post-tensioned concrete
    bridge decks? Apparently, due to the use of concrete
    that was late in arriving on site, inspectors suspect
    the occurrence of large entrapped air voids in the deck.

    Is UT the best test method for detecting these voids?
    Who in Eastern Canada has considerable experience with
    detecting such problems using UT?

    PCTE replied 2 years, 3 months ago 3 Members · 2 Replies
  • 2 Replies
  • Concrete Testing

    george

    Member
    28/11/2021 at 5:54 pm

    Our company has a system to inspect concrete for voids, cracks and thickness.
    Please call me at 416-213-8000 in Toronto

  • Concrete Testing

    PCTE

    Member
    03/09/2022 at 3:03 pm

    For such problem best option will be ultrasonic concrete testing equipment. They are NDT and best for your situation!