    Laminations are typically nothing more than a squashed bubble in the material. I’m assuming since your pipe is 60″ Diameter that it is seamed pipe formed from rolled plate and not extruded. The plate forming process is what turns a bubble in an ingot into a lamination. Also why they are commonly at a depth of half the thickness of the material.

Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.