NDT Community News Feed
Latest NDT & inspection industry news, jobs and community updates
Live updates from the NDT Inspect community: new NDT job vacancies, product launches from the virtual exhibition, forum discussions and member activity across ultrasonic, radiographic, phased array and every other inspection method. Join free to post and follow.
Sign in to post updates and join the conversation.
-
S.NOOR DEEN joined as Standard Member4 months ago -
NexxisUS joined as Standard Member4 months ago
-
AlexMcdurmon joined as Standard Member4 months ago
-
Rijo Ruban joined as Standard Member4 months ago -
SNS became a registered member4 months ago
-
Samuel Polonec joined as NDT Professional4 months ago -
Mali joined as Standard Member4 months ago
-
PAUT2257 joined as NDT Professional4 months ago
-
Jeetborescope joined as Standard Member4 months ago
-
Moein Rezaei joined as Standard Member4 months ago -
Vinay Kushwaha joined as Standard Member4 months ago -
samrn8 joined as Inspector4 months ago
-
Carolina Pena joined as Standard Member4 months ago -
Habeeb Rahman joined as Standard Member4 months ago -
pgr380 started the discussion Submerged Coatings DFT Inspection4 months ago
Coating: Modified Polyamine Epoxy
Application: Submerged service; wastewater treatment plant clarifiers
Currently inspecting new submerged coating (Tnemec 66 and 141) for dry film thickness. Specification calls for 4-6 mils primer and 10-15 mils top coat. So total DFT requirement is 14-21 mils. Some of the coating is applied to the inside and outside of a 10 ft diameter drum (open on top and bottom). The remainder is applied to angle iron fabricated into a truss like structure 80 ft long.
There is no spec for testing DFT's other than the implication that any DFT reading cannot be less than 14 mils which is probably unreasonable. However, applying SSPC PA2 (5 avg readings over 100 sq ft) to the drum seems inadequate to me for submerged coatings and since we've had quality control problems with the painter. Any advice on how to tighten up PA2 to catch areas of low DFT's?
Also, PA2 doesn't seem practical when testing small surface areas (such as angle iron). I've proposed taking 4 or 5 readings for each length along each face of each angle (generally 6-8 ft) and averaging that. Any thoughts?
Thanks -
pgr380 became a registered member4 months ago
-
svishwa Svishwa joined as NDT Engineer5 months ago -
Jayakrishnan P.K joined as NDT Professional5 months ago -
Muthu Kumar joined as Standard Member5 months ago -
AnthonyAguirre published a resume, Ndt inspector5 months ago
-
AnthonyAguirre became a registered member5 months ago
-
brycegraham joined as Standard Member5 months ago -
Surinder Surinder joined as Standard Member5 months ago -
Chinthala Manoj joined as Standard Member5 months ago -
Fardeen Khan joined as Standard Member5 months ago